logo
Home Cases

3169K UV Adhesive Case Study: Fixing BMS Components In Lithium Battery Packs With 5s LED Curing

Certification
China Shenzhen Super- curing Opto-Electronic CO., Ltd certification
China Shenzhen Super- curing Opto-Electronic CO., Ltd certification
Customer Reviews
We have cooperation for long long time ,it's a good experience .

—— Mike

Sincerely hope to we can cooperation next time soon.

—— Bok

I like your leduv flashlight very much it's hand-held and operation very easy.

—— Christophe

The UV lamp greatly improves the efficiency of our screen printing machine, it's great!

—— Alfie

The UV Curing Unit quality is excellent; I've used it for over a year without any problems.

—— Oliver

This lamp is perfect for curing silkscreen printing on our packaging. I love it.

—— Ethan

The UV LED curing lamps from this company are incredibly stable. We use them for our touch-screen bonding line, and the curing consistency is perfect.

—— David

They customized the perfect 365nm UV curing solution for our automated optical manufacturing line.

—— Elena

I'm Online Chat Now

3169K UV Adhesive Case Study: Fixing BMS Components In Lithium Battery Packs With 5s LED Curing

November 14, 2026
Latest company case about 3169K UV Adhesive Case Study: Fixing BMS Components In Lithium Battery Packs With 5s LED Curing

3169K UV Adhesive Case Study: Component Fixing in Lithium Battery Packs

How one adhesive change cut BMS fixing time from 45 seconds to 12 seconds and vibration failures from 2.1 to 0.3 percent

The result first: a battery pack plant replaced a solvent adhesive with 3169K single component UV adhesive and cut per board fixing time from 45 seconds plus 24 hours drying to 12 seconds with immediate handling. Vibration test failures fell from 2.1 percent to 0.3 percent. The curing lamp matters for takt time, but the failure was caused by the adhesive, and the adhesive is where the engineering effort went.

What Went Wrong With the Old Adhesive

The plant bonds relay supports, shunt holders and connector blocks onto BMS boards before potting, roughly 300,000 packs a year. The solvent adhesive failed in three ways:

  • It cured by evaporation, so parts could move for hours. Handled boards arrived at the potting station misaligned.
  • Its solvent attacked the solder mask, leaving white halos around the bond line.
  • Twenty four hours of rack drying locked up work in process and about 60 square metres of floor.

None of these was a lamp problem. Each traced back to how the adhesive cured and how it behaved on the substrate, which is why the evaluation focused on chemistry, viscosity and strength data rather than on curing hardware.

Why 3169K Was Chosen

3169K is a single component polyurethane acrylate that cures on UV or visible light exposure and needs no mixing. Four properties decided the selection.

1. Viscosity 12,000 mPa·s Fits the Dispensing Window

Too thin and the adhesive runs onto gold pads and under neighbouring parts; too thick and it bridges the component instead of wetting its edge. At 12,000 ± 1,500 mPa·s 3169K dispenses from a standard time pressure valve, stays where it is placed and flows into the 0.3-0.5mm gap along the component edge. The plant kept its existing valve and nozzle, so no capital cost was involved.

2. Shore D 80 and 13 MPa Hold Under Vibration

BMS boards face road vibration, drop testing and connector insertion force. A soft adhesive lets the component creep; a brittle one cracks at the fillet. 3169K cures to Shore D 80 with 13 MPa tensile strength, which is rigid enough to hold a relay support yet tough enough to absorb impact, and it keeps that performance through aging rather than embrittling in service.

3. Shear Strength on Aluminum and PC

The board carries an aluminum busbar and PC connector housings, two substrates that rarely share the same adhesive. Measured shear strength is more than 4 MPa on PC/PC and more than 7 MPa on PC/aluminum, so one grade covers both joints. This removed the second adhesive the plant used to keep for metal parts.

4. Electrical Safety Next to Sense Wires

Adhesive runs centimeters from live sense wires and shunts. 3169K gives 20 kV/mm dielectric strength with dielectric constant 2.4 and dielectric loss 0.03 at 1MHz, so it insulates without disturbing measurement. The cured layer is also colorless and transparent, letting inspectors confirm coverage instead of pulling parts to check.

The Curing Lamp: A Supporting Role

3169K needs light to reach the bond line, so the plant mounted a 200W 395nm UV LED lamp from the same supplier on the existing fixture at a 30-50mm working distance. Five seconds of exposure delivers about 6000 mJ/cm² at 2mm bond line thickness, which matches the 12 second takt. The lamp replaced a 4000W mercury unit on that station mainly because it starts instantly and adds no heat next to the cells; the adhesive choice is what fixed the failure mode.

ParameterValue
Lamp used200W UV LED, 395nm, 30-50mm distance
Exposure5 seconds
Accumulated energy6000 mJ/cm² at 2mm

Results After Three Months

IndicatorBeforeAfter
Fixing cycle time45s plus 24h drying12s, handle immediately
Vibration failure rate2.1 percent0.3 percent
Solder mask defectsWhite marks at bond lineNone observed
Adhesive grades in stockTwo, plastic and metalOne, 3169K
Floor space for racksAbout 60 square metresReleased to assembly

Three Points Worth Copying

  1. Diagnose the failure mode before buying hardware. Here the adhesive cured by evaporation, so no lamp upgrade could have solved it.
  2. Judge an adhesive by viscosity, hardness, shear strength and dielectric data on your own substrates, not by cure speed alone.
  3. Then match the lamp to the adhesive, and verify irradiance with a UV meter at the real working distance.

Request a Similar Evaluation

Send your substrate pair, component size, bond line thickness and takt time. Our engineers will confirm the 3169K grade and dispensing parameters, and specify the UV LED lamp only after the adhesive is settled.

Contact Details
Shenzhen Super- curing Opto-Electronic CO., Ltd

Contact Person: Mr. Eric Hu

Tel: 0086-13510152819

Send your inquiry directly to us (0 / 3000)